Through hole plating

Dec 15, 2008 0 Replies

Has anyone got any more details on the device pictured in

formatting link



- the original site appears to be down, and the wayback machine is having trouble retrieving the site... It looks build-able, if only more details (the chemistry being used, the times, the temperatures of the baths, etc.)



Looking at

formatting link
it seems that powdered graphite is a reasonable first stage for preparing the board for copper- plating, and it's a happy side-effect that the drill rubs the graphite into the hole when it withdraws from the hole.



Alternatively, anyone had any experience with the LPKF 'contac rs' or 'miniContac rs' machines ? And how much were they ?